Mixed Interlaminar Fracture Toughness and Durability of Composites under Humid and Hot Conditions
Table 1
Water absorption of the material after immersion in water for 7 days (10-2 g/cm3).
| Material temperature | 22°C | 60°C | 100°C |
| Epoxy resin | 0.24 | 0.39 | 1.12 | Glass fiber-reinforced composites | 0.13 | 0.24 | 0.68 | Carbon fiber-reinforced composites | 0.24 | 0.33 | 0.82 | Aramid fiber-reinforced composites | 0.48 | 0.68 | 4.78 |
|
|