Research Article
Properties and Modification of Bismuth-Layered Structure Ferroelectric Materials and Application in Sports
Table 8
Crystal information and refinement conditions of Bi4Ti3O12 at room temperature.
| | Atom | Site | | | | 100Uiso/A2 | Occupancy |
| | Bil | 4a | 0.25 | 0.7726 (14) | 0 | 0.95 | 0.505 | | Lal | 4a | 0.25 | 0.7726 (14) | 0 | 0.95 | 0.495 | | Bi2 | 8b | 0.244 (9) | 0.7266 (9) | 0.21672 (8) | 1.05 | 0.757 | | La2 | 8b | 0.244 (9) | 0.7266 (9) | 0.21672 (8) | 1.05 | 0.243 | | Bi3 | 8b | 0.248 (8) | 0.7804 (8) | 0.10695 (10) | 1.09 | 0.952 | | La3 | 8b | 0.248 (8) | 0.7804 (8) | 0.10695 (10) | 1.09 | 0.018 | | Ti1 | 8b | 0.252 (19) | 0.257 (4) | 0.0586 (4) | 0.19 | 0.75 |
|
|