Degradation and release of nanofibers in vitro. (a) SEM diagram of the degradation process of PLGA and PLGA/FK506 nanofibers at the 1 week, 3 weeks, and 5 weeks. (b) Degradation rate of the two nanofibers after 5 weeks. (c) Standard release curves of FK506. (d) Drug release process of the PLGA/FK506 nanofiber membrane.