Research Article
IoT-Based Intelligent System for Internal Crack Detection in Building Blocks
Table 1
Cube strength for 7 days and detected crack sizes.
| S. no. | Load in | 7-day cube compressive strength in N/mm2 | Cracks in mm |
| 1. | 50 | 2.22 | 0.00 | 2. | 75 | 3.33 | 0.00 | 3. | 100 | 4.44 | 0.15 | 4. | 125 | 5.56 | 0.20 | 5. | 150 | 6.67 | 0.30 | 6. | 175 | 7.78 | 0.30 | 7. | 200 | 8.89 | 0.75 | 8. | 250 | 11.11 | 0.75 | 9. | 275 | 12.22 | 1.00 | 10. | 300 | 13.33 | 1.00 | 11. | 325 | 14.44 | 1.75 | 12. | 358 | 15.91 | 2.50 |
|
|