Cylinder strength for 28 days and detected crack sizes.
| S. no. | Load in | 28-day splitting tensile strength in N/mm2 | Cracks in mm |
| 1. | 25 | 0.35 | 0.00 | 2. | 50 | 0.71 | 0.00 | 3. | 75 | 1.06 | 0.05 | 4. | 100 | 1.41 | 0.10 | 5. | 125 | 1.77 | 0.30 | 6. | 150 | 2.12 | 0.50 | 7. | 175 | 2.48 | 1.15 | 8. | 200 | 2.83 | 2.65 | 9. | 225 | 3.18 | 3.15 | 10. | 254 | 3.59 | 3.50 |
|
|