Effect of Nanoaluminium Nitride Ceramic Particles on Microstructure, Mechanical Wear, and Machining Behavior of Al-Si-Mg Alloy Matrix Composites Produced by Bottom Pouring Type Stir Casting Route

Table 1

Input parameters and output results.

Ex. NoCS (rpm)FR (mm/rev)DOC (mm)MRR (g/min)SR (μm)

110000.050.20.0731.88
210000.150.30.0971.68
310000.250.40.1181.75
420000.050.30.0812.02
520000.150.40.1042.25
620000.250.20.1242.09
730000.050.40.092.17
830000.150.20.1121.59
930000.250.30.1471.80