Ex. NoNormalized S/N ratioDeviation sequence
MRRSRMRRSR

100.56060610.439394
20.3243240.8636360.6756760.136364
30.6081080.7575760.3918920.242424
40.1081080.3484850.8918920.651515
50.41891900.5810811
60.6891890.2424240.3108110.757576
70.229730.1212120.770270.878788
80.52702710.4729730
910.68181800.318182