Growth of InAs(Bi)/GaAs Quantum Dots under a Bismuth Surfactant at High and Low Temperature

Figure 7

Integrated PL intensity from QDs (closed symbols) at 900 mW excitation plotted against bismuth flux. Values have been normalized to the maximum intensity which was recorded for layer H2. Values for the LEF in each layer have also been added (open symbols).