Investigation on Hot Corrosion Behaviour of Inconel 625 and Incoloy 800H Superalloys with YSZ-Thermal Barrier Coating Under High-Temperature Environment for Bioreactor Applications
Figure 20
XRD results of Inconel 625 specimens. (a) Uncoated 8-hour-heated. (b) YSZ-coated 8-hour-heated. (c) Uncoated 12-hour-heated. (d) YSZ-coated 12-hour-heated. (e) Uncoated 16-hour-heated. (f) YSZ-coated 16-hour-heated.