Journal of Nanomaterials / 2022 / Article / Tab 1 / Research Article
Morphological, Structural, and Optical Properties of Doped/Codoped ZnO Nanocrystals Film Prepared by Spin Coating Technique and Their Gas Sensing Application Table 1 Structural parameters of ZnO.
(hkl) 2θ (0 ) FWHM Cos θ (nm)Lattice spacing (nm) Antimony-doped ZnO (001) 23.38 0.563 0.979 14.29 0.339 (110) 28.39 0.403 0.929 20.17 0.180 (101) 39.80 0.348 0.940 24.07 0.202 (102) 41.65 0.347 0.934 24.30 0.153 (103) 51.33 0.357 0.901 21.96 0.098 Aluminum- and antimony-codoped ZnO (100) 31.70 0.667 0.961 16.28 0.449 (001) 34.37 0.524 0.955 17.21 0.205 (101) 36.23 0.466 0.950 20.23 0.301 (102) 47.49 0.428 0.915 24.21 0.177 (110) 56.56 0.388 0.880 24.96 0.153 (103) 62.79 0.351 0.853 25.03 0.123 (112) 68.01 0.344 0.829 27.40 0.099 (201) 69.10 0.328 0.826 27.68 0.095