Research Article

Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting

Figure 1

Squeeze casted specimen: (a) Ti-6Al-4V with 10 wt% WC composites; (b) Ti-6Al-4V with 15 wt% WC composites.