Research Article

Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting

Figure 3

Squeeze casting microstructure of (a) Ti-6Al-4V with 5 wt% of WC and (b) Ti-6Al-4V with 10 wt% of WC.
(a)
(b)