Research Article
Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting
Table 4
Wear rate values of Ti-6Al-4V matrix with 10% WCp (sliding distance 1000 m).
| Applied load | Ti-6Al-4V matrix with 10% of WCp | Ti-6Al-4V matrix with 15% of WCp |
| 10 | 11.848 | 16.848 | 20 | 13.156 | 18.156 | 30 | 15.9735 | 20.9735 | 40 | 17.099 | 22.099 | 50 | 19.407 | 24.407 | 60 | 21.042 | 26.042 | 70 | 23.331 | 28.331 | 80 | 25.683 | 30.957 |
|
|