Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting

Table 5

Wear rate values of Ti-6Al-4V matrix with 15% WCp (sliding distance 1000 m).

Applied loadTi-6Al-4V matrix with 10% of WCpTi-6Al-4V matrix with 15% of WCp

1022.84828.848
2024.15631.156
3026.973533.9735
4027.09936.099
5029.40739.407
6032.04242.042
7034.33145.331
8037.68347.957