Research Article
Microstructure and Mechanical Behaviour of Ti-6Al-4V Matrix Reinforced with WCp Developed by Squeeze Casting
Table 7
values of Ti-6Al-4V matrix with 15% WCp (sliding distance 2000 m).
| Applied load | Ti-6Al-4V matrix with 10% of WCp | Ti-6Al-4V matrix with 15% of WCp |
| 10 | 0.468 | 0.52 | 20 | 0.568 | 0.578 | 30 | 0.596 | 0.635 | 40 | 0.628 | 0.72 | 50 | 0.695 | 0.785 | 60 | 0.778 | 0.8469 | 70 | 0.84 | 0.924 | 80 | 0.88 | 0.9556 |
|
|