Research Article

Nanosilica-Based Teff Straw as an Eco-Friendly Substitute for Special Concrete

Table 4

Results on flexural strength.

Mixing codeSample no.Load failure in KNFlexural strength in MPa

M019.484.74
28.664.33
Mean9.074.54

M119.204.60
212.466.23
Mean10.835.42

M218.144.07
210.795.40
Mean9.474.73

M319.404.70
28.864.43
Mean9.134.57