Research Article
Investigation on Mechanical Durability Properties of High-Performance Concrete with Nanosilica and Copper Slag
Table 3
Impact of nanosilica on chloride penetration.
| Parameters | Charge passed (Coulombs 28 days) | Chloride penetration | Charge passed (Coulombs 90 days) | Chloride penetration |
| | 1140 | Low | 1155 | Low | | 1138 | Low | 990 | Extremely low | | 1050 | Low | 920 | Extremely low | | 980 | Extremely low | 850 | Extremely low | | 820 | Extremely low | 702 | Extremely low | | 910 | Extremely low | 788 | Extremely low | | 955 | Extremely low | 824 | Extremely low |
|
|