Research Article

Organic Template-Free Synthesis of Mesoporous ZnO Microparticles by Sol-Gel Method and Low-Temperature Hydrothermal Treatment

Figure 1

XRD patterns for mesoporous samples of ZnO in different temperatures, 100°C (AZN100), 120°C (AZN120), and 140°C (AZN140).