Research Article
Evaluation on Powder Metallurgy Process Parameters of Ball-Milled AA8079-B4C Nanostructured Composites via Taguchi Grey Relational Analysis
Table 3
Response table normalized SN ratios.
| Expt. no | Normalized S/N ratios | | Microhardness | Compressive strength |
| 1 | 0.403538 | 0.306989 | 2 | 0.454799 | 0.432618 | 3 | 0.104053 | 0.528704 | 4 | 0.491712 | 0.398203 | 5 | 0.516924 | 0.664992 | 6 | 0.761666 | 0.558398 | 7 | 0.538097 | 0 | 8 | 0.03162 | 0.772042 | 9 | 0 | 0.788488 | 10 | 0.367043 | 0.042028 | 11 | 0.727539 | 0.083448 | 12 | 0.326508 | 0.699102 | 13 | 0.109068 | 0.113598 | 14 | 0.221619 | 0.619004 | 15 | 0.586154 | 0.752855 | 16 | 0.130937 | 0.165829 | 17 | 0.553838 | 0.544084 | 18 | 0.275665 | 0.649764 | 19 | 0.681711 | 0.514086 | 20 | 0.192227 | 0.22339 | 21 | 0.743279 | 0.255672 | 22 | 0.460649 | 0.63743 | 23 | 1 | 0.681133 | 24 | 0.648001 | 0.784986 | 25 | 0.545341 | 0.604386 | 26 | 0.85778 | 0.898432 | 27 | 0.632539 | 1 |
|
|