Research Article

Reconnoitring Wear Resistance and Mechanical Strengths of AA8111/B4C/ZrO2 Nanocomposite through Taguchi Route

Table 2

AA8111/B4C/ZrO2 nanocomposite synthesizing variables and levels.

Input levels
S. No.Composites and testing parameters1234

1.Stir time (min) (ST)20253035
2.Melting temperature (°C) (MT)800850900950
3.Stir speed (rpm) (SS)400450500550
4.Nanoparticle reinforcement (%) (NPR)36912