Research Article

Reconnoitring Wear Resistance and Mechanical Strengths of AA8111/B4C/ZrO2 Nanocomposite through Taguchi Route

Table 4

Signal-to-noise ratios for the observations of wear test.

LevelNanoparticle reinforcement (%)Stir speed on the melt (rpm)Time duration of stirring (min)Melting temperature (°C)

110.45912.2319.0815.674
210.2717.28910.5966.037
35.4187.3017.94012.514
46.5335.8615.0658.456
Delta5.0406.3695.5316.840
Rank4231