Research Article

Reconnoitring Wear Resistance and Mechanical Strengths of AA8111/B4C/ZrO2 Nanocomposite through Taguchi Route

Table 5

Analysis of variance (wear test).

SourceDFSeq SSContributionAdj SSAdj MS value value

Regression40.3886669.51%0.388660.097176.270.007
Reinforcement of nanoparticles10.0968717.32%0.096870.096876.250.030
Stirring speed10.0989417.69%0.098940.098946.380.028
Stirring duration10.0710312.70%0.071030.071034.580.056
Melting temperature10.1218221.79%0.121820.121827.860.017
Error110.1704930.49%0.170490.01550
Total150.55915100.00%