Research Article
Reconnoitring Wear Resistance and Mechanical Strengths of AA8111/B4C/ZrO2 Nanocomposite through Taguchi Route
Table 7
Optimization process results (wear test).
| Solution | Reinforcement (%) | Stirring speed | Stirring time | Melting temperature (°C) | Wear rate (mm3/m) fit | Composite desirability |
| 1 | 4 | 400 | 20 | 950 | 0.0245325 | 1 |
|
|