Coded coefficients for hardness response with various A-TIG process parameters.
| Term | Coef | SE coef | T-value | P-value |
| Constant | 87.67 | 2.44 | 35.91 | 0.001 | Welding speed | −3.13 | 1.50 | −2.09 | 0.091 | Voltage | −1.62 | 1.50 | −1.09 | 0.327 | Current | −1.50 | 1.50 | −1.00 | 0.362 | Welding speed × welding speed | −1.58 | 2.20 | −0.72 | 0.504 | Voltage × voltage | 0.42 | 2.20 | 0.19 | 0.857 | Current × current | −2.33 | 2.20 | −1.06 | 0.338 | Welding speed × voltage | 0.00 | 2.11 | 0.00 | 1.000 | Welding speed × current | −1.25 | 2.11 | −0.59 | 0.580 | Voltage × current | 0.75 | 2.11 | 0.35 | 0.737 |
|
|