Intensity Loss of ZnO Coated on Fiber Optic

Figure 3

SEM image cross-section sample. (a) ZnO1, (b) ZnO2, and (C) ZnO3 on the fiber optic sphere with a size of 500x magnification, image thickness of ZnO nanoparticles coating scanned on spherical section, and image layer of ZnO nanoparticles on optical fiber surface scanned from the optical fiber surface.
(a)
(b)
(c)