Research Article

Photocatalytic Degradation of Phenol Using Immobilized Nanotube Photocatalysts

Figure 6

Photocatalytic performance of different silica gel loading in the phenol degradation. Conditions: TiO2 nanotubes and colloidal silica in the catalyst were 0.12 and 0.80 g/L, respectively, air flow rate = 0.3 L/min, initial phenol concentration = 30 mg/L, and medium pH = 3.
904629.fig.006