Mechanical properties of some natural fibers when compared with conventional E-glass.
| Fibers | Density (g/cm3) | Tensile strength (MPa) | Young’s modulus (GPa) | Elongation-at-break (%) | Reference |
| Hemp | 1.14 | 690 | 30–60 | 1.6 | [18] | Jute | 1.3–1.45 | 393–773 | 13–26.5 | 1.16–1.5 | [19] | Flax | 1.50 | 345–1100 | 27.6 | 2.7–3.2 | [19] | Pineapple | 1.56 | 170 | 62 | — | [20] | Cotton | 1.51 | 400 | 12 | 3–10 | [21] | Coir | 1.25 | 220 | 6 | 15–25 | [21] | Sisal | 1.33 | 600–700 | 38 | 2-3 | [21] | E-glass | 2.5 | 2000–3500 | 70 | 2.5 | [18, 19] | S-glass | 2.5 | 4570 | 86.0 | 2.8 | [19] | Carbon (standard) | 1.4 | 4000 | 230–240 | 1.4–1.8 | [19] |
|
|