Thermal properties of SF/rPP composites.
| Samples | (°C) | (°C) | (°C) | % Weight remaining at | Residue at 500°C |
| Neat rPP | 301.88 | 323.01 | 379.79 | 37.85 | 4.044 | UT40/rPP | 274.45 | 293.70 | 370.90 | 33.02 | 3.413 | T40/rPP | 271.30 | 294.69 | 351.97 | 51.54 | 3.327 | T40/MAPP/rPP | 262.64 | 281.83 | 350.39 | 44.70 | 2.943 | T40/MAPP/C1/rPP | 262.80 | 285.75 | 351.89 | 45.91 | 4.748 | T40/MAPP/C3/rPP | 265.76 | 288.27 | 352.54 | 45.91 | 8.919 | T40/MAPP/C5/rPP | 282.11 | 306.87 | 394.14 | 36.64 | 16.83 |
|
|