Synthesis of Gold Nanoparticles Using Tannin-Rich Extract and Coating onto Cotton Textiles for Catalytic Degradation of Congo Red
Table 2
Tearing strength values of fabric samples.
| Sample | Tearing strength (N) | Warp | Weft |