Research Article

Spin Speed and Duration Dependence of TiO2 Thin Films pH Sensing Behavior

Figure 6

Surface roughness of TiO2 sample spun at (a) 1000 rpm, (b) 2000 rpm, (c) 3000 rpm, and (d) 4000 rpm.
(a)
(b)
(c)
(d)