Research Article
Effect of Annealing on PL Intensity of NaYF4:Er3+, Yb3+/Ca2+ Phosphor and the Application to Temperature Sensor
Table 1
Comparison of key indicators between in other works and mine.
| Compounds | Range (K) | λEx (mn) | SA (% K−1) | SR (% K−1) | References |
| Er3+-Yb3+:YPO4@core | 303–463 | 980 | 4.95 × 10−3 | 0.43 at 463 K | [43] | CaTiO3:Er3+-Nd3+-Yb3+ | 303–573 | 980 | 5.10 × 10−3 | 0.84 at 386K | [44] | Ln2LiSbO6:Bi3+, Sm3+ | 298–498 | 320 | 1.52 × 10−3 | 1.48 at 498 K | [45] | GdVO4:Yb3+, Er3+ | 300–453 | 375 | 0.77 × 10−3 | 1.17 at 300K | [46] | NaYF4:Er3+, Yb3+/Ca2+ | 303–453 | 980 | 2.44 × 10−3 | | This work | NaYF4:Er3+, Yb3+/Ca2+ | 303–723 | 980 | 3.39 × 10−3 | 0.16 at 723 K | This work |
|
|