Research Article
Cleaning of Graphite Particles Embedded in the Surface of Ductile Iron by Using a Novel Method
Table 2
Designed laser cleaning parameters.
| Nominated name | Power (W) | Repetition rate(kHz) | Diameter of spot(mm) | Scanning rate(mmsā1) | Pulse duration (ns) | Pass |
| S0 | 200 | 15 | 0.5 | 3200 | 100 | 1 | S1 | 220 | 15 | 0.5 | 3200 | 100 | 1 | S2 | 240 | 15 | 0.5 | 3200 | 100 | 1 | S3 | 260 | 15 | 0.5 | 3200 | 100 | 1 | S4 | 280 | 15 | 0.5 | 3200 | 100 | 1 | S5 | 290 | 15 | 0.5 | 3200 | 100 | 1 | S6 | 290 | 15 | 0.5 | 3200 | 100 | 3 | S7 | 290 | 15 | 0.5 | 3200 | 100 | 5 | S8 | 300 | 15 | 0.5 | 3200 | 100 | 1 | S9 | 320 | 15 | 0.5 | 3200 | 100 | 1 | S10 | 320 | 15 | 0.5 | 3200 | 100 | 3 | S11 | 340 | 15 | 0.5 | 3200 | 100 | 1 |
|
|