Preparation and Performance of Vanadium Tailings-Reservoir Sediment-Phosphogypsum-Based Foamed Concrete
Table 3
Physical properties of OPC.
| Fineness (residue on 80 μm sieve) (%) | Normal consistency (%) | Setting time (min) | Stability | Flexural strength (MPa) | Compressive strength (MPa) | Initial setting | Final setting | 3 d | 28 d | 3 d | 28 d |
| 22.13 | 27.2 | 118 | 190 | Qualified | 5.3 | 8.8 | 32.5 | 59.7 |
|
|