Research Article
Effect of Ta Additions on the Microstructure, Damping, and Shape Memory Behaviour of Prealloyed Cu-Al-Ni Shape Memory Alloys
Figure 5
Stress-strain curves of Cu-Al-Ni-xTa SMAs loaded and unloaded at 200°C and then preheated to 300°C. (a) Cu-Al-Ni and Cu-Al-Ni-xTa SMAs with various Ta content: (b) 1.0, (c) 2.0, and (d) 3.0 wt.%.
(a) |
(b) |
(c) |
(d) |