Research Article

Corrosion Resistance of Waterborne Epoxy Resin Coating Cross-Linked by Modified Tetrabutyl Titanate

Figure 4

Nyquist plots of coatings after 10 days of immersion (a, b) and 30 days of immersion (c, d).
(a)
(b)
(c)
(d)