Research Article

Characterization of Retained Austenite in Advanced High-Strength Steel

Table 2

RA types and volume fraction in the three test specimens.

SpecimensTotal volume fraction of RA by X-ray measurementIsland-type RA by EBSD measurementThin film-type RA by calculation

1% Mn0.5%0.44%0.06%
1.4% Mn0.9%0.77%0.13%