Research Article
Kalman Filter-Based Multitype Measurement Data Fusion for Stress Intensity Factor Evaluation in Marine Structures
Table 7
SIF curve of cracks with different lengths during loading.
| Loading force (kN) | SIF | | | | | True value | KF | True value | KF | True value | KF | True value | KF |
| | 38.406 | 31.338 | 54.238 | 49.448 | 61.258 | 37.013 | 69.368 | 47.363 | | 75.437 | 65.794 | 108.401 | 101.015 | 122.549 | 101.524 | 137.956 | 111.638 | | 112.381 | 103.773 | 162.757 | 148.281 | 183.944 | 164.540 | 201.856 | 184.472 | | 150.168 | 144.244 | 216.870 | 205.604 | 245.308 | 234.317 | 271.659 | 259.369 | | 187.834 | 185.400 | 271.245 | 266.088 | 306.450 | 303.470 | 339.939 | 333.865 | | 224.312 | 226.208 | 325.216 | 326.992 | 367.691 | 371.713 | 406.255 | 407.069 |
|
|