Research Article

Variability of Dynamic Properties of Rubber Compounds for Elastomeric Bearings

Table 3

λ-factors for HDRs from experimental data, material test limits (bracketed), and annex J of [3].

Experimental data and (EN 15129 §8.2.2.1)EN 15129 annex J

GξGξ
LBUBLBUB

Temperature50°C0.82 (0.80)0.87 (0.80)
40°C0.88 (0.80)0.91 (0.80)
0°C1.301.181.151.10
−10°C1.52 (1.80)1.23 (1.8)1.251.09
−20°C−(1.80)1.26 (1.8)
−30°C−(1.80)1.53 (1.80)1.561.20

Ageing1.00 (1.00)1.18 (1.20)1.00 (1.00)0.86 (0.80)1.201.00

Frequency0.94 (0.80)1.16 (1.20)0.93 (0.80)0.91 (0.80)

Repeated cycles0.90 (0.80)1.18 (1.35)0.95 (0.80)1.09 (1.00)

Production variability0.95 (0.80)1.07 (1.20)1.00 (0.80)1.00 (0.80)

Values calibrated from data and in compliance with EN 15129 prescriptions.