Research Article
Preliminary Study on the Fabrication of Particulate Fuel through Pressureless Sintering Process
Figure 7
Scanning electron micrographs of the samples sintered at 1150°C for 80 min: (a) sample A (+50 mesh), (b) sample B (50~70 mesh), (c) sample C (70~100 mesh), and (d) sample D (100~170 mesh).
(a) |
(b) |
(c) |
(d) |