Research Article
Progressive Damage Process and Failure Characteristics of Coal under Uniaxial Compression with Different Loading Rates
Figure 7
Failure process of samples at different loading rates (the indicated stress is the axial stress at the corresponding loading moment): (a) 0.002 mm/min; (b) 0.004 mm/min; (c) 0.006 mm/min; (d) 0.008 mm/min; (e) 0.01 mm/min.
(a) |
(b) |
(c) |
(d) |
(e) |