Performance Degradation of Subsea Shield Tunnel Segment Accounting for Concrete Strength Loss and Steel Bar Corrosion
Figure 11
Degradation characteristics of the segment after 60 days of steel bar corrosion: (a) the displacement cloud during cracking and (b) the maximum principal stress cloud during cracking.