Research Article
Performance Degradation of Subsea Shield Tunnel Segment Accounting for Concrete Strength Loss and Steel Bar Corrosion
Figure 6
The relationship between strain energy and axial strain under different confining pressures: (a) group A samples under 4 MPa confining pressure, (b) group A samples under 8 MPa confining pressure, (c) group B samples under 4 MPa confining pressure, (d) group B samples under 8 MPa confining pressure, (e) group C samples under 4 MPa confining pressure, and (f) group C samples under 8 MPa confining pressure.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |