Research Article
Study of the Dynamic Mechanical Properties of Recycled Concrete Containing Ferronickel Slag Subjected to Impact
Table 2
Physical properties of cement.
| | Specific surface area (m2/kg) | Water requirement of standard consistency (%) | Setting time (min) | Stability | Flexural strength (MPa) | Compressive strength (MPa) | | Initial setting time | Final setting time | 3 d | 7 d | 28 d | 3 d | 7 d | 28 d |
| | 345 | 28.1 | 193 | 253 | Qualified | 4.98 | 6.97 | 9.35 | 24.02 | 40.27 | 51.03 |
|
|