Research Article
Study of the Dynamic Mechanical Properties of Recycled Concrete Containing Ferronickel Slag Subjected to Impact
| | Material | Ed (MPa) | Poisson’s ratio | ρ (kg·m−3) | σ0 (MPa) | τc (MPa) |
| | C3D8R (mortar) | 22,300 | 0.20 | 2310 | — | — | | C3D8R (recycled aggregate) | 47,200 | 0.23 | 2539.5 | — | — | | COH3D8 (recycled aggregate) | 47,200 | 0.23 | 2539.5 | 35.62 | 53.43 | | COH3D8 (mortar) | 22,300 | 0.20 | 2310 | 15.10 | 22.65 |
|
|