Research Article
Study on Lateral Deformation and Failure Characteristics of Coal Based on Different Confining Pressures
Table 1
Physical and mechanical parameters of coal samples under different confining pressures.
| Number | Loading rate (mm/min) | Diameter (mm) | Height (mm) | Confining pressure (MPa) | Peak strength (MPa) | Peak lateral strain, 10–2 | Peak axial strain, 10–2 | Maximum lateral strain, 10–2 | Maximum axial strain, 10–2 |
| M1 | 0.05 | 49.28 | 98.32 | 0 | 12.80 | 0.7667 | 0.5351 | 2.0611 | 0.997 | M2 | 0.05 | 49.42 | 98.89 | 3 | 43.95 | 0.6984 | 1.2775 | 1.6062 | 2.0216 | M3 | 0.05 | 49.3 | 100.18 | 5 | 53.36 | 0.852 | 1.2412 | 2.6946 | 2.1174 | M4 | 0.05 | 49.34 | 100.11 | 7 | 67.43 | 1.0649 | 1.8067 | 2.1468 | 2.3674 |
|
|