Research Article

Experiment and Failure Analysis of Rock-Like Material Affected by Different Excavation Depths

Figure 19

Failure diagram of specimen with single-hole crack: (a) H = 0 mm, (b) H = 20/40 mm, and (c) H = 60/80/100 mm.