Research Article
Compressive Test Characteristics and Constitutive Relationship of Wet Polypropylene Macrofiber-Reinforced Shotcrete
Table 3
Initial strength attenuation coefficients of three different shotcrete mixes.
| Specimen code | Dry shotcrete | Wet shotcrete | Wet polypropylene macrofiber shotcrete |
| 1 | 0.860 | 0.719 | 0.877 | 2 | 0.723 | 0.665 | 0.571 | 3 | 0.672 | 0.799 | 0.696 | 4 | 0.805 | 0.757 | 0.650 | 5 | 0.850 | 0.836 | 0.551 | 6 | 0.909 | 0.682 | 0.658 | Average | 0.803 | 0.743 | 0.667 |
|
|