Research Article
Experimental Study on Mechanical Damage and Fracture Characteristics of Granite under Different Water Cooling Conditions
Figure 9
Micro failure characteristics of granite treated by different temperature drops and thermal cycles. (a) Room temperature, (b) temperature drop of 10°C, 4 cycles, (c) temperature drop of 10°C, 8 cycles, (d) temperature drop of 10°C, 12 cycles, (e) temperature drop of 15°C, 12 cycles, (f) temperature drop of 20°C, 12 cycles.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |