Research Article

Static and Dynamic Tensile Mechanical Behavior of Polyvinyl Chloride Elastomers with Different Shore Hardness

Table 1

Table 1Changes in dynamic tensile parameters.

57  A52 A47 A
760 s−11100 s−11450 s−1760 s−11200 s−11800 s−1400 s−1700 s−1950 s−1

Secant modulus (MPa)61.8895.48119.6181.9090.85250.5189.78115.62134.82
Peak stress (MPa)8.4313.3819.028.9718.1240.409.1913.2517.99
Peak strain (%)24.1025.3745.7417.0032.9154.2014.1216.0726.85