Research Article

Seismic Performance of Concrete-Filled Square Steel Tubular Column-Steel Beam Sleeve Joint

Table 2

Performance parameters of steel.

Thickness (mm)Measured strength (MPa)Average strength (MPa)

5.65Yield strength323.86322.72323.29
Ultimate strength474.09473.42473.76
7.65Yield strength299.50282.88291.19
Ultimate strength390.05392.82391.43
9.67Yield strength313.57319.68316.62
Ultimate strength420.86427.45424.15